Plastics — Differential scanning calorimetry (DSC) — Part 5: Determination of characteristic reaction-curve temperatures and times, enthalpy of reaction and degree of conversion
Primary tabs
This document specifies a method for the determination of reaction temperatures and times, enthalpies of reaction, and degrees of conversion using conventional differential scanning calorimetry (DSC) as specified in ISO 11357-1.
The method applies to monomers, prepolymers, and polymers in the solid or liquid state. The material can contain fillers and/or initiators in the solid or liquid state.
This document is not applicable to fast DSC as specified in ISO 23976.[
1 ]