Rigid PVC pipes — Differential scanning calorimetry (DSC) method — Part 2: Measurement of the enthalpy of fusion of crystallites
Primary tabs
Reference:
ISO 18373-2:2008
Publication Year:
2008
ISO 18373-2:2008 specifies a method for the determination of the enthalpy of fusion of crystallites in rigid PVC pipe samples. The method is based on the measurement of the thermal history using differential scanning calorimetry (DSC) and is suitable for all types of rigid PVC pipes.