Specification and qualification of welding procedures for metallic materials — Welding procedure test — Part 4: Finishing welding of aluminium castings
Primary tabs
Reference:
ISO 15614-4:2005
Publication Year:
2005
Domain:
ISO 15614-4:2005 specifies how a welding procedure specification for finishing welding of aluminium castings is qualified by welding procedure tests. It does not apply to repair welding.